Skip to main content
. 2021 Dec 15;13(24):4396. doi: 10.3390/polym13244396

Figure 9.

Figure 9

XPS C 1s, O 1s, and N 1s high-resolution spectrum components and their atomic concentrations for the water-washed plasma-treated PP samples. Spectra were measured right after washing.