Skip to main content
. 2021 Dec 10;13(24):4324. doi: 10.3390/polym13244324

Figure 8.

Figure 8

The relationship between mobile amorphous (χmaf) and strain at break for annealed PLA after the 1 h hydrolysis at 70 °C and 95% RH.