Skip to main content
. 2021 Dec 14;13(24):4372. doi: 10.3390/polym13244372

Table 6.

Simulation results of the Strehl ratio that considered the tolerances of the mold in the cases of wearing glasses.

Surface Tolerance (%) Anterior Radius (Ry) (mm) Posterior Radius (Ry) (mm) Strehl Ratio
P407DA/PHEMA Biconic +1 7.48208 6.57005 0.139
±0 7.408 6.505 0.857
−1 7.33392 6.43995 0.142
Aspherical +1 7.48107 6.59833 0.029
±0 7.407 6.533 0.496
−1 7.33293 6.46767 0.046
Spherical +1 7.50228 6.54379 0.034
±0 7.428 6.479 0.403
−1 7.35372 6.41421 0.084
P407DA/PAA Biconic +1 7.59116 6.11252 0.14
±0 7.516 6.052 0.86
−1 7.44084 5.99148 0.142
Aspherical +1 7.64772 6.92052 0.031
±0 7.572 6.852 0.499
−1 7.49628 6.78348 0.051
Spherical +1 7.67095 6.88618 0.033
±0 7.595 6.818 0.371
−1 7.51905 6.74982 0.092