Skip to main content
. 2021 Dec 9;13(24):4301. doi: 10.3390/polym13244301

Figure 4.

Figure 4

The XPS surface composition versus treatment time in ammonia plasma: (a) 200 W, continuous treatment (b) 200 W, pulsed treatment and (c) 25 W, continuous treatment. All samples were pretreated with hydrogen plasma at 35 Pa, 600 W for 1 s.