Skip to main content
. 2021 Dec 17;14(24):7836. doi: 10.3390/ma14247836

Figure 2.

Figure 2

Etching results for samples of the milled thin-film module made of CdTe in 1 M H2SO4, 3 M HNO3, and 30% H2O2 at (A) 30 °C and (B) 50 °C.