Skip to main content
. 2021 Dec 8;24(3):231–235. doi: 10.4103/jcd.jcd_29_21

Table 1.

Intergroup test of significance for resin-modified glass ionomer cement, nanohybrid and compomer using unpaired t-test at different intervals

Group Preinstrumentation
Postinstrumentation
Postpolishing
Group I (manual scaling) Group II (ultrasonic scaling) Group I (manual scaling) Group II (ultrasonic scaling) Group I (manual scaling) Group II (ultrasonic scaling)
Resin modified GIC
 Mean±SD 0.11±0.05 0.14±0.09 0.18±0.05 0.49±0.20 0.12±0.04 0.16±0.09
 Mean difference −0.02 −0.31 −0.04
t-test −0.721 −4.665 −1.344
P 0.480 0.001* 0.196
Nanohybrid composite
 Mean±SD 0.14±0.08 0.12±0.09 0.24±0.15 0.14±0.07 0.15±0.05 0.13±0.02
 Mean difference −0.02 −0.10 −0.02
t-test 0.471 1.879 1.009
P 0.643 0.077 0.326
Compomer
 Mean±SD 0.12±0.04 0.09±0.04 0.23±0.08 0.13±0.05 0.13±0.05 0.10±0.05
 Mean difference −0.03 −0.10 −0.03
t-test 1.518 3.511 1.192
P 0.146 0.002* 0.249

*A significant difference at 0.05 level of significance (P<0.05). SD: Standard deviation