Skip to main content
. 2021 Dec 30;13:100198. doi: 10.1016/j.mtbio.2021.100198

Fig. 3.

Fig. 3

(a) Photothermal properties of P-PPor NPs at various concentrations upon 808 ​nm laser (1.5 ​W/cm2) irradiation; (b) Photothermal properties of P-PPor NPs upon laser with different power densities; (c) Photothermal properties of P-PPor NPs after five on/off irradiation cycles; (d) Linear cooling time data versus ln(θ) of P-PPor NPs in the cooling period; Absorption spectra before and after radiation of ICG (e) and P-PPor NPs (f).