Skip to main content
. 2021 Aug 18;29(3):4497–4507. doi: 10.1007/s11356-021-15923-x

Fig. 2.

Fig. 2

Concentrations of PFOS in μg/g adsorbed on different size particles of PE (4–6; 11–13; 20–25; and 250–500 μm) after exposure to 25, 50, 75, and 100 μg/L of PFOS for 7 days. Mean ± SD; n=3