Skip to main content
. 2021 Dec 29;15(1):248. doi: 10.3390/ma15010248

Table 3.

Selected parameters for the thermal decomposition process for polystyrene.

Parameters of Thermal Decomposition PS-0 PS-1
Initial decomposition temperature [°C] 260.0 280.2
End temperature of 1st stage of decomposition [°C] 424.0 433.3
Loss of weight for 1st stage of decomposition [%] 98.0 92.1
Temperature of loss of 50% of weight [°C] - 404.6
Maximum rate of weight loss [%/min] - 18.2
Temperature of maximum rate of weight loss [°C] 392.0 412.1
Maximum rate of weight loss for 2nd stage [%/min] - 0.7
Temperature of maximum rate of weight loss for 2nd stage [°C] - 526.0
Residual mass [%] 2.0 1.4