. 2021 Dec 28;12(1):71. doi: 10.3390/nano12010071

Table 1.

Comparison of diffraction angles (in degrees) for rings or spots for carbon-based materials measured at 30 keV. The experimental data are from C 100 nm thin foil diffraction maxima, Figure 8, and graphene diffractogram from reference [57] (Figure 6).

“Order”\Source C 100 nm, 2D-PAD Graphene Bragg Formula (hkl)
“1st” 1.0 - 1.0 (100)
“2nd” 1.7 1.8 1.7 (110)
“3rd” 3.0 3.1 2.9 (300)