Skip to main content
. 2021 Dec 22;12(1):19. doi: 10.3390/nano12010019

Figure 6.

Figure 6

Logarithm of room-temperature forward current density as a function of logarithm absolute voltage for the MIS structures with ZnO:N films, deposited at Ar:O2:N2 = 50:10:40 (sample 2.1) and after RTA at 550 °C (sample 2.3).