Skip to main content
. 2021 Dec 13;12(1):101–115. doi: 10.1021/acscatal.1c04205

Figure 3.

Figure 3

Effect of the temperature on the accelerated degradation tests (ADTs) performed at the potential window of 0.6–1.0 VRHE (comparing RT and 75 °C, 5000 cycles, 1 V s–1, 0.1 M HClO4) comparing (a) ECSACO loss, (b) SA loss, and (c) Co loss of the ReCatalyst intermetallic dealloyed Pt–Co/C electrocatalyst. Comparison of the CO-electrooxidation CVs as well as the follow-up cycles before and after the ADT performed at (d) RT and at (e) 75 °C. Comparison of the ORR polarization curves before and after the ADT performed at (f) RT and at (g) 75 °C.