Table 5.
Active Agent | Processing Technique | Release Conditions | Diffusion Coefficient (m2 s−1) |
References |
---|---|---|---|---|
Merkén | Extrusion | EtOH 50% at 40 °C | 2.0 × 10−13 | [43] |
Thymol | Extrusion | EtOH 95% at 40 °C | 6.0 × 10−13 | [12] |
Solvent Casting | EtOH 10% at 40 °C | 2.5 × 10−13 | [46] | |
Supercritical impregnation | EtOH 10% at 40 °C | 1.5 × 10−13 | [15] | |
EtOH 95% at 40 °C | 2.8 × 10−11 | |||
Cinnamaldehyde | Electrospinning | EtOH 50% at 40 °C | 1.0 × 10−12 | [42] |
Supercriticalimpregnation | 6.0 × 10−14 | |||
Casting (PLA monolayer) | EtOH 50% at 20°C | 6.3 × 10−14 | [79] | |
Thermo-compression (PLA-bilayer) |
9.0 × 10−15 |