Skip to main content
. 2012 Aug 13;83(3):425–430. doi: 10.2319/052212-419.1

Figure 6.

Figure 6.

Lased HF specimen showing glazed or slightly melted appearance with absence of smear layer, laser-induced pitting or cavitation, linear cuts/markings, carbonization of surface, or heat-induced surface cracking. Bar  =  10 µm at an original magnification of (a) 50× and (b) 750×.