. 2022 Jan 18;31(1-2):145–158. doi: 10.1007/s11666-022-01320-4

Fig. 1.

Fig. 1

Particle size distribution of coarse powder (10 to 45 µm), As-Received, and heat-treated (C-AR: As-Received, C-HT 600 °C: heat-treated at 600 °C, C-HT 875 °C: heat-treated in a rotary tube furnace at 875 °C)