Skip to main content
. 2022 Jan 18;31(1-2):145–158. doi: 10.1007/s11666-022-01320-4

Fig. 10.

Fig. 10

PSD of fine H13 powder before (F-AR) and after HT 875 °C under argon atmosphere and cooled at 350 °C/h in pure argon (F-HT 875 °C-4)