Skip to main content
. 2022 Jan 18;31(1-2):145–158. doi: 10.1007/s11666-022-01320-4

Fig. 11.

Fig. 11

Microstructures (BSE, 15kV, 1000X ) of a H13 deposit sprayed using F-HT 875 °C-4 powder (HT under argon atmosphere and cooled at the rate of 350 °C/h)