Skip to main content
. 2022 Jan 18;31(1-2):145–158. doi: 10.1007/s11666-022-01320-4

Fig. 3.

Fig. 3

Microstructures (BSE, 15kV, 500X) of deposits produced with H13 coarse powder (a) C-AR (b) C-HT 600 °C (c) C-HT 875 °C