Fig. 8.

Fig. 8

Sankey chart depicting the pyrolysis mass balances of the respective pure virgin polymers pyrolyzed in a fixed-bed batch reactor at 700 °C, based on (Williams and Williams, 1997b). For the sake of comparability, the reported mass balances by were normalized to 100 %.