Tabularized representation of the results from the post-hoc Tukey’s HSD test for differences between means of the shear bond strength in particular samples defined by ceramics and cement type. The samples are sorted according to the means in ascending order. The means that are not significantly different from each other form a homogenous group and are marked by three black dots (“●●●”) in the same column. All means that do not share dots in the same column are significantly different from each other.

Cement Ceramics Shear Bond Strength [MPa] Homogenous Groups
Mean SE 1 2 3 4 5 6 7
RelyX U200 IPS e.max ZirCAD 1.95 0.158 ●●●
Maxcem IPS e.max CAD 2.06 0.159 ●●●
Maxcem IPS e.max ZirCAD 2.32 0.158 ●●● ●●●
Panavia SA IPS e.max ZirCAD 2.55 0.158 ●●● ●●● ●●●
Panavia SA IPS Empress CAD 2.98 0.163 ●●● ●●● ●●●
RelyX U200 IPS e.max CAD 3.14 0.159 ●●● ●●●
Panavia SA IPS e.max CAD 3.21 0.159 ●●● ●●●
RelyX U200 IPS Empress CAD 3.36 0.163 ●●●
Maxcem IPS Empress CAD 3.37 0.163 ●●●
Panavia V5 IPS e.max ZirCAD 7.60 0.158 ●●●
Panavia V5 IPS Empress CAD 16.84 0.163 ●●●
Panavia V5 IPS e.max CAD 19.45 0.159 ●●●