The fitting parameters of impedance spectra at various temperatures for the glass-ceramic prepared at 490 °C for 12 h.

Sample 490 C-12 h Equivalent Circuit Parameters
Temperature R (Ω) CPE 1 CPE 2
A1 (sα Ω−1) α 1 A2 (sα Ω−1) α 2
−30 °C 1.14 × 1012 3.61 × 10−12 0.76 - -
0 °C 3.78 × 1010 8.52 × 10−12 0.74 - -
30 °C 1.65 × 109 2.21 × 10−11 0.74 - -
60 °C 2.17 × 108 3.87 × 10−11 0.74 2.78 × 10−7 0.34
90 °C 3.27 × 107 6.58 × 10−11 0.73 1.14 × 10−6 0.39
120 °C 6.28 × 106 1.03 × 10−10 0.73 3.50 × 10−6 0.47
150 °C 2.12 × 106 1.52 × 10−10 0.72 3.89 × 10−6 0.63
180 °C 5.39 × 105 1.91 × 10−10 0.72 7.42 × 10−6 0.56
210 °C 1.85 × 105 2.65 × 10−10 0.71 1.35 × 10−5 0.55
240 °C 7.08 × 104 3.09 × 10−10 0.72 1.79 × 10−5 0.53