. 2022 Jan 12;15(2):567. doi: 10.3390/ma15020567

Figure 10.

Figure 10

SEM fractography images of the alloy ZK60 specimen fatigued to fracture in air: (a) overview of the fracture surface (a) and a magnified view of the crack initiation site (b), pointed to by a red arrow in (a).