Skip to main content
. 2022 Jan 12;15(2):567. doi: 10.3390/ma15020567

Figure 11.

Figure 11

SEM images of the fracture surface after testing in Ringer’s solution with 50 MPa at 10 (a,c,e) and 80 Hz (b,d,f); initially ground surface (a,b), polished surface (c,d), and Zr-coated surface (e,f).