(a) FT-IR spectra of AHPCS and PVZ. (b) TGA plots recorded between room temperature and 1000 °C under inert atmosphere on PVZ and AHPCS, DCP-PVZ and DCP-AHPCS, PLA molds coated with preceramic polymers i.e., PLA/DCP-PVZ and PLA/DCP-AHPCS.