(a,b) Simulated voltage profiles of Li/LLZO/LCO all-solid-state battery at different C rates (0.001C, 0.2C, 0.5C, 1C, 2C, and 5C) and temperatures (30 °C and 70 °C), using cathode constant areal capacity of 4 mAh cm−2 and LLZO thickness of 30 µm. (c,d) Gravimetric and volumetric Ragone plots of Li/LLZO/LCO solid-state battery simulated using cathode areal capacities of 0.5, 1, 2, 3, 4, and 5 mAh cm−2 at temperatures of 30 °C and 70 °C and constant LLZO thickness of 30 µm. The simulations were performed using LCO cathode that is composed of 70 vol.% of LCO and 30 vol.% of LLZO.