Skip to main content
. 2022 Jan 24;12:1253. doi: 10.1038/s41598-022-05412-7

Figure 8.

Figure 8

Deformation characteristics of SM products: (a) the CNC machined module showed no change after EO sterilisation (0–1), while severe deformation appeared after autoclaving (0–2); (b) the injection moulded product showed no change after EO sterilisation (9–1), while severe deformation appeared after autoclaving (9–2).