Skip to main content
. 2021 Aug 17;26(1):939–955. doi: 10.1007/s00784-021-04077-2

Fig. 9.

Fig. 9

Representative XRD patterns of NC, SB, LC, LR and LW zirconia groups. a) SB showed clear m-ZrO2 peaks and smaller t-ZrO2 peaks, whereas NC showed the highest intensity peak for t-ZrO2 peak (30.17 degrees). b) All laser treated groups showed similar XRD patterns and in none of them an increase of monoclinic phase could be detected. In addition, SB showed a broadened tetragonal peak (arrow). c) Tetragonal peak intensity inversion after SB