Skip to main content
. 2022 Jan 11;7(3):3121–3133. doi: 10.1021/acsomega.1c06714

Table 1. Comparison of Photodegradation Efficacies between Zi-AuNPs and Other Photocatalysts against MG.

catalyst dye concentration (ppm) degradation efficiency (%) time (min) ref
CuFe2O4 18 62.37 210 (47)
ZnO 5 49 60 (48)
ZnO modified with EDTA 94.14
CdSe/TiO2 10 99 360 (49)
chitosan-supported ZnO 5 ∼100 90 (50)
Pd/WO3 photocatalyst 5 66.66 360 (51)
Au–ZnO nanofilm 10 76.92 240 (52)
Zi-AuNPs 25 81.14 100 current study
50 63.29