. 2022 Jan 29;20:55. doi: 10.1186/s12951-022-01262-7

Fig. 3.

Fig. 3

A UV–vis absorption of ZnS NPs, ICG and ICG-ZnS NPs. B ICG loading capacity and encapsulation efficiency of ICG-ZnS NPs in different mass ratio of ICG/ZnS NPs. C, D Temperature profile of different concentrations of ICG-ZnS NPs (1 W·cm−2). E H2S release performance of ICG-ZnS NPs with different pH. F Zn2+ release performance of ICG-ZnS NPs with different pH