Figure 10.

Figure 10

T1 results of the degradation of PLA nanoparticles containing 70 nm FNDs before and after degradation at pH 4.5 for 1 day at 1 μM Gd3+. The data were analyzed using Student’s t test, and statistical significance was accepted at *P ≤ 0.05 and **P ≤ 0.01.