Skip to main content
. 2022 Jan 21;23(3):1200. doi: 10.3390/ijms23031200

Figure 7.

Figure 7

Magnetization curves for the multicomponent PLGA based delivery system (PLGA_IO-OA_OXA) and its PEGylated analog (PEGylated PLGA_IO-OA_OXA) before and after dissolution tests measured at room temperature (25 °C) in the magnetic field from −10 kOe to +10 kOe.