. 2022 Feb 8;15(3):1248. doi: 10.3390/ma15031248

Figure 6.

Figure 6

IPFs maps of plane A at (a) RT, (b) 400 °C, and (c) 550 °C of 9Cr-F/M steel and the histogram of misorientation angle of Z0 direction corresponding to each above.