Skip to main content
. 2022 Jan 25;27(3):776. doi: 10.3390/molecules27030776

Figure 8.

Figure 8

The effect of the precursor solution’s pH on the (a) crystallite size, (b) specific surface area and pore volume, (c) BJH pore size distribution, and (d) band gap of the synthesized NiMoO4 materials. Calcination temperature: 500 °C, calcination time: 6 h, and φ = 1.