Table 2.
Parameters and results of orthogonal experiment
Scheme No. | HA content A (%) | Layer thickness B (mm) | Printing speed C (mm/s) | Filament feeding speed D (mm/s) | Bending strength (MPa) |
---|---|---|---|---|---|
1 | 0 | 0.1 | 30 | 0.7 | 97.2±7.85 |
2 | 0 | 0.15 | 40 | 0.8 | 82.1±4.81 |
3 | 0 | 0.2 | 50 | 0.9 | 11.7±0.35 |
4 | 10 | 0.1 | 40 | 0.9 | 96.2±4.58 |
5 | 10 | 0.15 | 50 | 0.7 | 30.9±12.86 |
6 | 10 | 0.2 | 30 | 0.8 | 80.4±8.08 |
7 | 20 | 0.1 | 50 | 0.8 | 63.5±3.65 |
8 | 20 | 0.15 | 30 | 0.9 | 71.7±13.70 |
9 | 20 | 0.2 | 40 | 0.7 | 10.6±2.16 |