Pore-size distribution of chitosan cryogels prepared with different procedures based on mercury intrusion porosimetry (A). Nitrogen adsorption (closed)/desorption (open) isotherms of samples at 77.3 K (B) and pore size distribution curves calculated using the DFT method (C).