Table 1. Yield of Chitosan-Based Cryogels Obtained at 2.0 wt % Chitosan Loading Amount With Glutaraldehyde as the Crosslinker.
gel
yield (%) |
||||
---|---|---|---|---|
crosslinker content (vol %) | 1 | 2 | 3 | average ± standard deviation |
0.1 | 77.3 | 75.7 | 79.5 | 77.5 ± 1.6 |
0.2 | 80.4 | 77.0 | 80.8 | 79.4 ± 1.7 |
0.3 | 76.8 | 75.0 | 75.5 | 75.8 ± 0.7 |
0.4 | 80.1 | 83.4 | 79.7 | 81.1 ± 1.6 |
0.5 | 76.6 | 74.0 | 81.8 | 77.2 ± 2.9 |