Skip to main content
. 2022 Feb 19;27(4):1421. doi: 10.3390/molecules27041421

Table 2.

Electrochemical Corrosion Result.

Tested Samples and Hours Corrosion Potential(V) Corrosion Current Density Beta Anode
(V/Decade)
Beta Cathode
(V/Decade)
Rate of Corrosion (mpy)
1 h Immersion
PD-3
−1.0210325 1979.07 μA/cm2 0.6475 ± (0.01023) −0.544 ± (0.00725) 9.25 × 10−4 (±1%)
24 h Immersion
PD-1
−0.259503 2.25425 μA/cm2 0.08593 ± 7.9088 × 10−4 −0.20133 ± 0.00161 0.0343 × 10−4 (±1%)
48 h Immersion
PD-2
−0.583870009 12.38734 μA/cm2 0.06737 ± 8.3756 × 10−5 −1.1648 ± 0.00785 1.88 × 10−4 (±1%)