Figure 3.

Figure 3

(A) DSC curves of glycerol-plasticized silk films with various glycerol contents. The samples were heated from 0 to 250 °C with a heating rate of 10 °C/min. (B) The second scan DSC curves of glycerol-plasticized silk films with various glycerol contents. The first heating scan was from 20 to 200 °C with a heating rate of 20 °C/min for removing free water in the films and the second heating scan was from −30 to 220 °C with a heating rate of 20 °C/min. (C) Glass transition temperatures of glycerol-plasticized silk films with various glycerol contents.