Published in final edited form as: J Am Chem Soc. 2022 Feb 14;144(7):3285–3296. doi: 10.1021/jacs.2c00421

Figure 5.

Figure 5.

(a) Comparison with direct-insertion reactive alkyl iodide. SEM images of lyophilized zinc sample treated (b) with micelles and (c) in the absence of micelles. (d) Summary of EDS data by %/wt in samples.