Uniaxial tensile elongation of PE/iPP materials and blends. Materials were melt-blended at 190 °C without BCPs (black) or with 1 wt % diblock (green), 1 wt % tetrablock (orange), or 5 wt % tetrablock copolymers (purple). These materials were then compression molded into tensile specimens at 180 °C and tensile tested at a rate of 100%/min (Adapted with permission from the work of Eagan et al.35 Copyright 2017 AAAS).