TABLE 4.

Substrate characteristics of wood samples from parental and triploid willow genotypes and their positive and negative midparent heterosis (MPH%) values for cell wall components.

Genotypes Wood weight (g/cm) Acid detergent lignin(%) Cellulose +
cutin (%)
Hemicellulose
(%)
Tordis 0.62 ± 0.01 15.18 ± 1.06bc 41.81 ± 2.13a 18.33 ± 0.39b
TH3/12
MPH%
0.82 ± 0.07
14.25
13.89 ± 3.50c
–8.01
37.93 ± 3.29ab
–1.48
20.32 ± 0.42a
17.73
PP-E7 0.80 ± 0.08 15.02 ± 1.09bc 35.19 ± 0.76b 16.19 ± 0.54d
Tordis 0.62 ± 0.01 15.18 ± 1.06bc 41.81 ± 2.13a 18.33 ± 0.39b
TH17/17
MPH%
0.78 ± 0.05
7.57
18.09 ± 0.25ab
15.59
35.60 ± 2.01a
–6.68
18.10 ± 0.36b
–2.09
PP-E15 0.83 ± 0.01 16.12 ± 3.03abc 34.49 ± 2.25b 17.13 ± 0.24c
Inger 0.88 ± 0.22 19.17 ± 0.24
a
39.53 ± 3.07
ab
17.19 ± 0.30c
TH21/2

MPH%
0.92 ± 0.30

8.98
14.64 ± 1.64
bc
–14.36
38.68 ± 3.81
ab
3.53
16.19 ± 0.14d

–3.00
PP-E7 0.80 ± 0.08 15.02 ± 1.09bc 35.19 ± 0.76b 16.19 ± 0.54d

Results are mean ± SD. Values denoted with different letters show significant differences at p ≤ 0.05 (Duncan’s test). Bold values highlight the MPH% and CPH% information.