Skip to main content
. 2022 Feb 23;14(5):868. doi: 10.3390/polym14050868

Table 9.

Forest plot of the main discoveries on geopolymer concrete’s resistance to sulfuric acid, with reference to Table 7 and Table 8.

Published Work Compressive Strength of Geopolymer Concrete without Acid Exposure (MPa) Compressive Strength of Geopolymer Concrete with Acid Exposure (MPa) Compressive Strength Reduction (%) graphic file with name polymers-14-00868-i001.jpg
Abhilash et al. [67] 35.87 33.82 5.72
Valencia-Saavedra et al. [68] 42.92 34.34 20
Çevik et al. [69] 48.4 39.2 19
Average 14.91