Figure 4.

Figure 4

Flowchart showing the preparation of rGO LB film. To distribute the rGO flakes evenly, methanol vapor from a methanol-soaked tissue was applied to gently force the clouded regions apart to significantly improve the film uniformity. Reprinted with permission from ACS Publications, copyright 2015, American Chemical Society [34].