. 2022 Feb 22;14(5):858. doi: 10.3390/polym14050858

Table 1.

Crystallinity of investigated thin films after heat treatment.

Heat-Treatment Neat
P3HT:PCBM
P3HT:PCBM
+ 5% I2
P3HT:PCBM
+ 10% I2
non-annealed 36% 37% 39%
annealed at 100 °C 48% 49% 51%
annealed at 210 °C 46% 46% 49%