Figure 13.

Figure 13

(a) Effect of AC deposition percentage on photocatalytic dye degradation of RR 120 and OFL (AC-TiO2 suspended = 50 mg/100 mL; pH = 5; irradiation time = 50 min), (b) photodegradability of RR 120 with and without scavenger, AC-TiO2 suspended = 50 mg/100 mL; pH = 5; irradiation time = 50 min.