Table 2.
Characterization of nanoparticles assembled from PLA-PEG BBCPs in water
|
Z-average DLS hydrodynamic diameter.
Determined from cryo-TEM imaging (mean ± SD).
Obtained from static light scattering and Zimm plot analysis.