Table 4.
Corrosion parameters extrapolated from Tafel fit of potentiodynamic polarization plots for Ti6Al4V specimens.
Specimen | Ecorr (V) | Icorr (μA/cm2) | Bc (mV/dec) | Ba (mV/dec) |
---|---|---|---|---|
Forging | -.122 | 0.0176 | 94.5 | 261.2 |
EBM-V | -1.24 | 0.0311 | 85.4 | 162.9 |
EBM-H | -1.18 | 0.0113 | 84.3 | 176.8 |
SLM-V | 1.29 | 0.3428 | 88.1 | 223.5 |
SLM-H | 1.23 | 0.0833 | 84.3 | 352.9 |