. 2022 Mar 9;10(3):42. doi: 10.3390/dj10030042

Table 3.

Effect of thermocycling (before and after) and type of material on tested properties using two-way ANOVA.

Properties Variables Type III Sum of Squares df Mean Square F-Value p-Value
Water Sorption (µg/mm3) Materials 229.884 3 76.628 58.555 0.000 *
Thermocycling effect 707.455 1 707.455 540.600 0.000 *
Materials × thermocycling 36.850 3 12.283 9.386 0.000 *
Error 94.223 72 1.309
Total 37,813.148 80
Solubility (µg/mm3) Materials 0.805 3 0.268 11.072 0.000 *
Thermocycling effect 5.050 1 5.050 208.482 0.000 *
Materials × thermocycling 1.939 3 0.646 26.681 0.000 *
Error 1.744 72 0.024
Total 113.962 80
Translucency Materials 188.669 3 62.890 87.503 0.000 *
Thermocycling effect 174.434 1 174.434 242.701 0.000 *
Materials × thermocycling 2.540 3 0.847 1.178 0.324
Error 51.748 72 0.719
Total 5006.175 80

* Statistically significant at the 0.05 level.