Skip to main content
. 2022 Mar 9;24(3):386. doi: 10.3390/e24030386

Table A4.

Summary statistics of the Concrete Dataset.

Concrete Dataset
Variable Scales of Measurement Range Mean/Median Variance/IQR
Compressive Strength continuous [2.33;82.6] 35.82/34.45 279.08/22.43
Cement Component continuous [102;540] 281.17/272.9 10,921.58/157.625
Blast Furnance Slag Component continuous [0;359.4] 73.90/22 7444.125/142.95
Fly Ash Component continuous [0;200.1] 54.19/0 4095.62/118.3
Water Component continuous [121.8;247] 181.57/185 456/27.1
Super- plasticizer continuous [0;32.2] 6.205/6.4 35.67/10.2
Coarse Aggregate Component continuous [801;1145] 972.92/968 6045.68/97.4
Fine Aggregate Component continuous [594;992.6] 773.58/779.5 6428.19/93.05
Age in Days continuous [1;365] 46.66/28 3990.44/49