. 2022 Mar 13;14(6):1150. doi: 10.3390/polym14061150

Figure 1.

Figure 1

Effect of pre-heating treatment (40, 60, and 80 °C) on shear strength of plywood specimens in different conditions (dry, cold water soaking, and boiling water soaking). Control: Ambient temperature (20 ± 2). EN 314-2 specifies 1 N/mm2 for dry shear strength of plywood [32].